Dear If your procedure is for micro-molding and fabricate the SU-8 master. I suggest the exposure time down to 1/3. It has good adhession on glass but it will damage by acetone. C.M. Lin Microfluidics Lab, NTU,TW ----- Original Message ----- From: "annuar"To: Sent: Tuesday, June 15, 2004 8:55 AM Subject: [mems-talk] SU-8 adhesion to glass substrate > Hi everyone. > I'm having problem coating my glass slide with SU-8 resist. It seems that > the SU-8 does not adhere very well to glass. After developing, some part of > my patterns are lifted off. Does anyone know how to solve this problem? Does > the softbake or PEB have anything to do with this? Thanks. > > Abang Annuar > > > > >