Dear Robert, I'm sure you must have a reason for using NMP. People tend to use it as an acetone replacement to reduce fire hazards and it is reclaimable. No one uses it because it works so well. Can you use any common resist strippers or EKC's nophenol 922? Brent Robert Dean wrote: > Hello, > > We are ion milling a thin layer of Au/Cu on a polymeric substrate, while > using photoresist (AZ5124EIR) as the etch mask. The ion milling works very > well for etching the Au and Cu. However, the process results in > crosslinking of the photoresist where we cannot remove it from the > remaining Au/Cu traces on the substrate, even through heated NMP based > stripper baths for 20 hours. Unfortunately, ashing would damage the > polymeric substrate. Does anyone have a suggestion on how to remove the > remaining photoresist? > > Sincerely, > > Robert Dean > Auburn University > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/