Hi all,

I have questions about stress in thin film:

(1) what range of stress can cause reliability issues in microelectronics
thin film ? Is 500 MPa in a 0.5 um thick metal thin film a lot of stress to
cause undesired failure ?
(2) does compressive stress cause yielding like tensile stress does ?

Thanks !!!