Hello,

I have experimented with SU-8 layers patterned on BCB.  The adhesion at the
SU-8 / BCB interface varies from poor to awful.  Has anyone else tried this
before?  I've tried AP3000 as an adhesion promoter to no avail.

Thanks,
-M. A. Powers