Hi Han,

Dow Corning makes a silicone based paste containig ZnO2 that is commonly
used for this purpose.

Jobert van Eisden
School of Nanoscale Science and Engineering
University at Albany, NY

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org]On Behalf Of BobHendu@aol.com
Sent: Thursday, July 08, 2004 5:49 PM
To: mems-talk@memsnet.org
Subject: Re: [mems-talk] Question about thermal conductive glue for drie


We sometimes use Fomblin oil and it seems to help with heat spread. In a
message dated 7/8/2004 2:40:03 PM Eastern Daylight Time, "Han Geun Yu"
 writes:

>Hi, I am struggling with heat problem of substrate while doing drie.
Because I use small piece, I need carrier wafer to do drie and I think it
makes heat to flow little. If you know any glue or greese to increase the
heat flow, please let me know.
>
>Thank you.
>
>Han
>_______________________________________________
>MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply