Hi, Can anyone help me in finding 1) the best recipe for the wet etch for Platinum which can stand standard photoresist (AZ 4330). 2)Also, I want to create some rectangular shape (1mmx1mm) cavities of about 20 microns deep. Can anyone help me in this regard too. I've on my one wafer devices with metal combinations Pt/Ti and on other wafer devices Pt/Cr and third wafer with Ti/Cr. Will it be feasible to create cavities before or after fab process. Any suggestions will be appreciated. imran mi_ghauri@yahoo.com Grad Student __________________________________ Do you Yahoo!? New and Improved Yahoo! Mail - 100MB free storage! http://promotions.yahoo.com/new_mail