Hi Peggy, Is it possible for you to first create the pyramid structures on the silicon substrate and then deposit BST to create the array you desire. Phillipe Tabada >From: "WENYI ZHU">Reply-To: General MEMS discussion >To: mems-talk@memsnet.org >Subject: [mems-talk] need help on making pyramid array on the ceramic >thickfilm >Date: Mon, 26 Jul 2004 16:17:21 -0400 (EDT) > >Dear all, >I am trying to make some pyramid array on the ceramic thick film about 25 >micrometers to 100 micrometer thick.I found a method called anisotropic >etching in KOH can make pyramid cavity on the <100> single crystal si >wafer,but my etching object is isotropical ceramics,for example BST(Barium >strontium titanate).It is a kind of polycrystal material.Is there any other >method to make these pyramids in such fine scale? >You will be highly appreciated you if you can give me any suggestions. >Thanks a lot! > >peggy > >_______________________________________________ >MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk >Hosted by the MEMS Exchange, providers of MEMS processing services. >Visit us at http://www.memsnet.org/ _________________________________________________________________ Overwhelmed by debt? Find out how to Dig Yourself Out of Debt from MSN Money. http://special.msn.com/money/0407debt.armx