You can use Thermo Couple (TC) wafers to calibrate your wafer temp. You can
contact SensArray Corporation for TC wafers.

"Tan, Chuan Seng"  wrote:
Hi All,

Does anyone know how to determine the wafers temperature during metal
deposition in an e-beam chamber ?

Thanks for your inputs.

Chuan Seng