Dear Joe

The Resolution Performance Products web site ,
under "EPON - Multi-functional, Novolac, Elastomeric, and
Cycloaliphatic Resins", has this PDF has information for the typical
properties of SU-8:
http://www.resins.com/resins/am/pdf/SC1580.pdf

It lists a typical density of 10.0 lbs/gal.

In sensible units this is 1.20 g/cm3 or 1200 kg/m3.

I have not confirmed this density with any of our SU-8 batches.

Regards,

Chris Blanford

On Saturday, August 14, 2004, at 05:12 AM, Siripon Sukuabol wrote:

> Hi..All;
>
>
> Does anyone know about SU-8 Density?
> Where can I get this information?
>
> Regards;
>
> Joe

--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: +44 (0)1865 282603; Fax: +44 (0)1865 272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/