Michael Cooke
2004-08-16
I dont have experience of this exactly, but you could imerse it in bomb if
your other components will hold
Dr. Michael Cooke
Microsystems Technology Group
School Of Engineering
University of Durham
Durham
DH1 3LE
Phone: +44 (0)191 3342535
Fax:      +44 (0)191 3342407
Email:   m.d.cooke@physics.org
Webpage Http://www.dur.ac.uk/microsystems.technology
----- Original Message -----
From: "Erik Jung" 
To: "General MEMS discussion" 
Sent: Monday, August 16, 2004 10:25 AM
Subject: [mems-talk] Removal of reflowed AZ resist


> Dear all,
> anyone of you has experience in completely removing AZ photoresist after
> reflowing SnAg solder in the openings (Tmax~230?C, t@Tmax ~ 40sec)
> Thank you!
>
> Erik
> TU Berlin
>
>
>


reply