durusmail: mems-talk: Dissolving epoxy
Oxide Release - Etch Holes
2004-08-24
Dissolving epoxy
2004-08-25
Dissolving epoxy
Vikas Nair
2004-08-25
Hi,

I wish to remove the packaging of a 5 mm x 5 mm x 2 mm, 8-pad hermetic LCC
package without damaging the silicon n metal structures inside. Is there
any standard method to do this??....
Thanks

Vikas Nair
IITB



reply