Jeff, I thing that if you use a microscope with interference contrast you will be able to see the lines again. Brent Jeffrey Price wrote: > Hello, > > I am trying to diffuse Ti strips into Lithium Niobate. The strips run > from approximately 3 -10 um. After diffusion (which I have run > different permutations ranging from 1-9h and 900-1050C) in a wet > nitrogen environment the waveguides completely disappear. I know that > the index delta should be approximately .01 so they should be difficult > to see, but I can't seem to see anything at all. I was wondering if > anyone has had this problem before or can help me find a solution. Thanks. > > Jeff Price > Research Assistant, University of Delaware > price@ee.udel.edu > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/