2 microns is VERY thick for evaporated metal. It will probably crack. I wouldn't recommend evaporating anything over 1 microns thick, and even that may be tricky. -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Bravo Han Sent: Thursday, September 02, 2004 8:14 PM To: mems-talk@memsnet.org Subject: [mems-talk] Electroplating Gold vs. E-Beam Evaporation Gold Hi folks, To obtain a layer of Au that is not too thick, for example, just around 2 microns, are there any significant differences in the final metal film deposited by electroplating vs. the one by e-beam evaporation? Thanks for your attentions and inputs. _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/