durusmail: mems-talk: Some questions about ultrathick resist Jsr THB430N & SU8
Some questions about ultrathick resist Jsr THB430N & SU8
2004-09-07
Some questions about ultrathick resist Jsr THB430N & SU8
tida
2004-09-07
i searched the company website already and found nothing related to
this material.
And, i also send the enquiry email to the related department but no response .:(

Anyway to get this material other than buy from jsr corporation?

And does anyone using this material to make a mold before?
Is that really easy to form a thickness 1mm mold if compared with SU8?


SU-8:

How to coat su8 on the substrate in order to get rid of the air bubbles?
Because of the air bubbles, i redo the experiment many times already :(
I saw someone post before, he said dont use the pipet to draw the su8.
Then what else should i use?? *confuse*


Thanks in advance. :)

reply