Need advice from SU-8 experts:
I have 30um width by 55um height SU-8 2035 lines. Somehow, after 35s exposure
time and post-bake of 95oC for 20min, the resulting structures are tapered with
bottom 60um width and top 40um width. Can anyone offer possible solutions to
troubleshoot the problem?

Thanks!!