Venkatachalam Chokkalingam
2004-09-15
hai..

the details u r looking for are available at
http://www.memsnet.org/material/

You can look for SiO2 bulk, SiO2 ....

Bye,
Venkat...



--- Mihaela Miu  wrote:

> Hi All;
>
>
> Does anyone know about silicon oxide properties like
> density, Young's modul,
> Poisson ratio, or conductivity?
> Where can I get this information?
>
> Regards;
>
> Mihaela
>
> Mihaela Miu
> National Institute for Research and Development in
> Microtechnologies
> (IMT - Bucharest)
> Erou Iancu Nicolae 32B, 72996 Bucharest, Romania
> http://www.imt.ro 
> Phone: +40-21-490.84.12;
> Fax: +40-21-490.82.38
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>




__________________________________
Do you Yahoo!?
Yahoo! Mail is new and improved - Check it out!
http://promotions.yahoo.com/new_mail

reply