>it is very important to >cool the wafer during etching, then why not put wafer on the stainless steel >subtrate directly, why use He gas cooling? since steel have much higher >thermal conductivity than He gas. Because you operate in vaccum. Surface roughness of the wafer backside and the chuck prevent perfect thermal contact. Helium provides thermal contact between wafer and chuck.