let me relay you to my colleague gunter.engelmann@izm.fhg.de. He built a electrostatic motor with that technique. Radant MEMS www.radant.com are building RF switches in gold. Good luck! -----Ursprungliche Nachricht----- Von: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]Im Auftrag von Laetitia Philippe Gesendet: Donnerstag, 30. September 2004 16:47 An: mems-talk@memsnet.org Betreff: [mems-talk] MEMS in electroplated gold Hello everybody, is someone aware on the microfabrication of 18 carat gold object by electrodeposition? I don't find so far much infos about that many thanks for your help Dr Laetitia Philippe Electrochemistry and Micro-patterning Group EMPA Feuerwerkstrasse 39 CH-3602 Thun Tel 41 (0)332285249 _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/