Glass Frit can be obtained from Ferro Corporation in Clevland Ohio (USA) ,
phone (216) 641 -8580


> I'm a research student at the Technical University of Dresden, Germany,
working at a project
> about glass-frit bonding.
>
> For my practical research I need small amounts of glass-frit paste. Could
you perhaps tell me
> where I could find this, or its components, and how much it would cost me?
Furthermore, I
> would need to know about the conditions this paste fulfills. How does it
react to exposure to
> temperature or pressure? I read about kinds that react at 600C-800C,
others that react at
> about 290C-380C, and yet another reacting at above 100C. Would that be the
same paste
> or are totally different procedures applied?
> I would be very grateful if you could help me out with information,
sources in literature or
> ideas where to look.
>
>
> With best regards
>
> Genadi Genadiev
> genadiev@ihm.et.tu-dresden.de
>Request: END
>
>
>


reply