Hi, Would you please tell me the etch rate of Si-Nitride in BHF? Thanks Laleh Rabieirad PhD Student ECE Department Purdue University Quoting Peter Andreas Rasmussen: > Then your nitride is of poor quality - perhaps PECVD? I've measured the > ethcrate of Si-rich LPCVD sini in 5% BHF to 0.4 nm/min. (giving etch-rate > ratio between oxide and nitride of ~200!) > > regards, > Peter Andreas Rasmussen > Postdoctoral Research Fellow > MIC - Institute for Nano and Microtechnology > Technical University of Denmark > > Phone: (+45) 4525 5732 Mail: pra@mic.dtu.dk > http://www.mic.dtu.dk/ > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/ > >