selectively etch Gold in presence of Nickel and otherNickel alloys
2004-10-14
2004-10-14
2004-10-14
selectively etch Gold in presence of Nickel and otherNickel alloys
Hung-Ming Chen
2004-10-14
This might work,

KI/I2/H2O (4g:1g:40ml)

Hung-Ming Chen

--- Chen-Han Lee  wrote:

>
>
> Hi,
>
> could some one recommend some echant which etches
> gold but not Nickel or
> other nickel alloys.
>
> thanks for helping
>
> chen-han
>
> ///////////////////////////////////
> Chen-Han Lee
> Research Student
> School of Manufacturing and Mechanical Engineering,
> University of Birmingham,
> Birmingham, B15 2TT
> United Kingdom,
> Phone :  +44 121 4144245
> Fax :    +44 121 4143958
> E-Mail : dcl815@bham.ac.uk
> ///////////////////////////////////
>
>
> _______________________________________________
> MEMS-talk@memsnet.org mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>




_______________________________
Do you Yahoo!?
Declare Yourself - Register online to vote today!
http://vote.yahoo.com

reply