Are you sure? I look for another paper and get the Young's modulus of TaN is 150GPa~250GPa! So I don't know which one is correct. Anyone can tell me what value is correct? ----- Original Message ----- From: "Suhua Jiang"To: Sent: Friday, October 15, 2004 12:23 PM Subject: RE: [mems-talk] TaN > 455GPa > > >From: 童麒嘉 > >Reply-To: General MEMS discussion > >To: > >Subject: [mems-talk] TaN > >Date: Tue, 12 Oct 2004 19:36:07 +0800 > > > >Dear all, > > Anyone can tell me the Young's modulus of Tantalum nitride? > > Or any textbook can find this data? > > Thanks > > Rasheed > >_______________________________________________ > >MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > >options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > >Hosted by the MEMS Exchange, providers of MEMS processing services. > >Visit us at http://www.memsnet.org/ > > > National Microanalysis Center > Materials Science Department > Fudan University > 220# Handan Road > Shanghai, 200433 > China > Tel: 86-21-65642380 > > > _______________________________________________ > MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.memsnet.org/