durusmail: mems-talk: Dry etch mask
Dry etch mask
2004-10-29
Dry etch mask
William Lanford-Crick
2004-11-01
Nickel (with Cr or Ti adhesion layer) or NiCr should be good.
-Bill

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org]On Behalf Of Zhiyan Liu
Sent: Friday, October 29, 2004 5:06 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] Dry etch mask


Dear all,

Does anybody has an idea of the dry etch metal mask. The dry etched i used
are Cl2/BCl3.

Thank you ,

Zhiyan