COD. Catastrophic optical damage? Are talking about laser diodes?
-Jukka Viheriälä
"Booth, David"
cc:
Sent by: Subject: [mems-talk] Alumina
slurry
mems-talk-bounces@
memsnet.org
29.10.2004 19:33
Please respond to
General MEMS
discussion
I was wondering if anyone had any information about the contribution of a
polycrystalline alumina polishing slurry towards COD. We've seen that
relative to a colloidal silica for example, the alumina slurry leads to a
very high COD, and don't quite understand this. Any information would be
great, cheers.