durusmail: mems-talk: TMAH Etch Without Attacking Aluminum
TMAH Etch Without Attacking Aluminum
2004-11-22
2004-11-23
TMAH Etch Without Attacking Aluminum
Kevin Duan
2004-11-22
Hi, dear all

I am planning to do TMAH etching of silicon wafer with aluminum
pattern on it.  I want to achieve as low etch rate for Al as possible.
 Some people add some silicon powder and some other additive, like
amonium nitrate to do that.  Does anyone have some experience in doing
so?  How about the experimental setup and the condition?

Thanks ahead.

Duan

reply