Hi Lee, I would suspect that the thermal conductivity and electrical resistivity of the materials would influence the deposition rates. In case you use different boats for holding the tagets, material differences may also have an impact on the net thermal conductivity. -Mike >>> lsjun@phya.snu.ac.kr 12/6/2004 5:34:32 PM >>> Dear members, I'm a graduate student of Physics. I would like to know about the mechanism of power in the electron beam evaporator. We made a simple e-beam evaporator for metallization (Ti, Pt, and Pd) using 1mm diameter metal rod in the lab. As you may know well, the emission current determine the power in the evaporator. Strangely, I found the emission current of Ti is higher than that of Pd to get the same evaporating rate, even though the melting point of Ti is less than that of Pd . In my experience in MEMS instruments, the emssion current of Ti is very lower than that of Au. Could you how to explain this fact? As another question, I would like to know the behavior of metal rod (source). In the Pt case, the droplet was formed on top of the rod in evaporating. But Ti rod was bent after evaporating and Pd was formed the needle shape like SPM tip. Does anyone know about these things? Thank you in advance. Lee _______________________________________________ MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at http://www.memsnet.org/