I am trying to find the best exposure time for a SU8-2035 with a

thickness of around 50 um

This is not looking to be very easy. I am working with a UV i-line 365

nm, with 20 mW/cm2



For high exposure time (up to 100s ), I see that my structure does not

developp at all, i.e. the exposed polymer is not removed in the

developper although the sutructre is clearly visible with a color difference

between the exposed and non exposed part



For reasonnable exposure time (20 s), I have a good developpment but I

have always a resulting mould that is small as my mask. i.e some

feature of my pattern of 200 um would lead to only 100 um cavity in my

developped polymer and so one.



Finally, when I go down to 7 seconds, I have a good resulting mould,

with much better dimensions, but I have enormous stress on my polymer and

sometimes delamination which makes me thing I am under exposing of

course





Could someone share his own experience about that? especially about the

over-exposure'?



Many thanks