durusmail: mems-talk: Which kind of metal film will not be attacked or relatively much slower etched in TMAH
Which kind of metal film will not be attacked or relatively much slower etched in TMAH
2004-12-13
Which kind of metal film will not be attacked or relatively much slower etched in TMAH
Kevin Duan
2004-12-13
As subject.
I want to have a patterned metal film on silicon wafer, and don't want
the film be etched during the wet etching in TMAH.
Does anyone know which kind of metal can survive in TMAH?  I know
someone has succeeded in not attacking aluminum in TMAH.  But that
needs some additives, and with limited success.  So could you give
some suggestion?

Thanks very much.

reply