-----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Borski, Justin Sent: Thursday, December 16, 2004 9:50 AM To: 'General MEMS discussion' Subject: RE: [mems-talk] Elevated temperature acetone bath for metallic liftoff process Hi Thomas, You would be better served safety-wise by running an NMP-based process. You can safely run NMP solvent up to 70 degrees C without too much worry. And you should do this in an all-metal station. - Justin Justin, Thanks very much. I've ordered a liter of it from VWR and will try it Monday. Any advice on the temperature - the Cleanroom temperature is ~20 C or less. What do you mean by an all-metal station? I'm an external user at U-Del ECE's Cleanroom - their fumehoods are the white plastic that I suppose is resistant to HF and other acids (which I don't use myself). I will definitely not use the ultrasonic bath.