Dear LeiNie,

Normally a silicon dioxide mask is used for SiN wet etching because the
photoresist will not hold up.  Transene manufactures Transetch N for wet
etching silicon nitride; visit www.transene.com.

Regards,

Christopher Christuk
Transene Company