Hi I want to deposit Ni and Cobal layer 100 nm on Si by sputtering / E-beam evaporation process. Does any one has receipe for this ? what should be the power, deposition rate ?? -- Thanks, Pradeep Dixit Research Student, Micromachine Center, NTU Singapore - 639669