Hi All: What are the possible causes of a flickering plasma in an RIE system? We have an ICP-RIE system and the plasma flickers at any pressure above 4 mT or so. This was not observed in the system until the past few weeks, and the system is about 6 years old. I have cleaned the chamber thouroughly (flickering plasma in the past has been an indication of a dirty chamber) and yet the plasma still flickers at all but the lowest pressures. Also, it the system will glow with a dim, very unstable plasma at low power levels ( < 30 W RF1 ) even though the matching network tunes to 0 reflected power. Through manual tuning of the matching network, I can get a bright, much more stable plasma (also with 0 reflected power). This might be a sign of something wrong with the matching network and possibly unrelated, but I thought I'd mention it. Any thoughts on this are greatly appreciated! Bill Lanford University of Illinois Micro and Nanotechnology Laboratory