Hi Bill, Here are some possible causes of unstable plasma: 1) pressure too low to sustain the plasma 2) RF matching network is not working properly 3) metal contamination or some metal pieces that causes the power and ground electrodes to short. It looks like static discharge. 4) also, your power supply can be aging too. Yours sincerely, Isaac Chan University of Waterloo