Bill: Check out the water you are running thru your wafer chuck. Is it controlled by a chiller unit or house water. You might want to check the resistivity of the water. Above a certain point it can create what I call thunderbolts in the chamber. Just replace with distilled water and some ethylene glycol and the problem should resolve itself. Bob Henderson