Dear Haroon, Here is a link of an article where you can find all the relevant information: http://dx.doi.org/10.1016/j.optmat.2003.12.004 (joural site) http://www.fen.bilkent.edu.tr/%7Eay/publications/JOM_FAY.pdf (pdf file) You should pay attention on dilution of precursor gases, power, and flow rates and then adapt these parameters to your system. Regards, Feridun Ay Bilkent University