Bonding Kapton to glass
Bill Moffat
2005-01-26
Joe,
    Vacuum vapor prime with HMDS or APTES then spin on Polymide.  This should
adhere to Kapton an as it is cured at up to 450 C should withstand the
temperature.  Bill Moffat