Kory, I used 8" round gold targets that I indium bonded to water cooled backing plates. Depending on how much you are going to use this target will decide how thick to make it. Little use, 1/8", lot of use, 1/4" thick. I also sputtered Cr/NI/Au on the back side before bonding. Brent