> Date: Thu, 2 Apr 1998 19:43:31 -0600 (CST) > From: Stefano Ratti> Subject: Yttrium oxide emissivity > To: MEMS@ISI.EDU > Reply-to: Stefano Ratti , mems-cc@ISI.EDU > Does anyone know what the emissivity of the yttrium oxide is ?? > It should be temperature dependent. Does anyone have something like a > table with the values of the emissivity at different temperatures?? We own an Agema 900 thermographic system with microscope lens which we often use for thermal characterization of microsystems. Experience has shown that tabulated values of material emissivities are hardly usable in practice. As you may find in literature, various kinds of emissivity are defined and what you need uses to be a mixture of several values. It is therefore better to calibrate your system well and calculate the emittance. If you like, we can try to support you with our system. Yours sincerely, Kai Hiltmann mailto:Kai.Hiltmann@IMIT.Uni-Stuttgart.de http://www.IMIT.Uni-Stuttgart.de K. Hiltmann c.o. IMIT W.-Schickard-Str. 10 D-78052 Villingen-Schwenningen Tel. ++49-7721-943-236 Fax ++49-7721-943-210