durusmail: mems-talk: AZ4620 Removal after High temperature Bake
AZ4620 Removal after High temperature Bake
2005-03-09
2005-03-10
2005-03-14
AZ4620 Removal after High temperature Bake
Kasman , Elina
2005-03-10
Try AZ Kwik Strip - it's designed for AZ4620.
But after baking at this high temperature, I doubt you will be
successful...