durusmail: mems-talk: how to prevent the natural oxide formation on poly-Sifilm for tr
how to prevent the natural oxide formation on poly-Si film for transportation?
2005-03-20
how to prevent the natural oxide formation on poly-Sifilm for tr
2005-03-21
how to prevent the natural oxide formation onpoly-Sifilmfor tr
2005-03-21
how to prevent the natural oxide formation on poly-Sifilm for tr
li cai
2005-03-21
How thin is the film?  Dip in DILUTED HF may help.

>I have a sample with ultra-thin poly-Si film on the top to be transported.
>Does anybody know any ways to prevent the formation of the natural oxide
>layer on the poly-Si film during transportation?

reply