RE: Spam:[mems-talk] pinhole free metal film on glass substrate
2005-04-05
RE: Spam:[mems-talk] pinhole free metal film on glass substrate
Matthew Coda
2005-04-05
You may want to evaluate the smoothness of the glass surface, if it has
high aspect ratio asperities even with conformal metal coating they will
likely result in pinholes given enough subsequent processing steps.