Shane Arthur McColman
2005-04-06
Hi Eric,

A short SF6 etch in the RIE will get rid of it but etches other features more
than oxidizing will.  It's a good alternative if you can't survive the high
temperatures of oxidation

--
Shane McColman
Research Professional
NanoFab, University of Alberta