Hi Mallik, you can use a surface profilometer to measure topology. There are contact ones and non contact ones. My lab has a contact one that just drags a stylus over the surface being measured (this kind is called a stylus profilometer). hope that helps, Joe mallikarjun kamavaram wrote: >I WANT SOME ONE HELP ME IN COMPLETING MY PROJECT, >AM WORKING ON SANDBLASTING PROCESS, AND I HAVE DESIGNED micro/milli >CHANNELS ON GLASS AND I WANT TO KNOW HOW TO MEASURE THE DEPTH FO THE >CHANNELS I MADE ON GLASS. >I WANT SOME ONE TO TELL THE DEVICE OR METHOD WITH WHICH I CAN TAKE >MEASUREMENTS.