durusmail: mems-talk: Electrodeposition of Stainless Steel
Electrodeposition of Stainless Steel
Electrodeposition of Stainless Steel
laetitia philippe
2005-04-22
Hello All,

is someone aware of possibilities to deposit electrochemically FeNiCr alloys, in
such range of stainless steel composition?

I know only few papers from a group (from Hungary) able to deposit 1-2
micrometers thicks such alloys? does it exist something else, and more espcially
is someone aware of how to deposit thicker layer?

Thanks a lot
Carson