The most minimum thickness of SU8 spin coating?
The most minimum thickness of SU8 spin coating?
ajheim@mail.usf.edu
2005-04-24
If you heat the Su-8 to a near boil (I am sorry I can't get you a specific
temperature) it is possible to get very thin samples.  We have gotten
around 1 um before.  But it would be easier to use Shipley.

August
reply