durusmail: mems-talk: help on tungsten / tungsten silicide selective etch
help on tungsten / tungsten silicide selective etch
2005-04-26
help on tungsten / tungsten silicide selective etch
Jialin Zhao
2005-04-26
I am trying to find a selective etchant for W and WSix. The tungsten is
sputtered on silicon, and rapid thermal annealed to form a few nanometers of
silicide. To remove the unreacted W without etching the underlying
silicide, what wet etching could be used?
Thanks
--
Jialin Zhao
204 Cushing Hall
Department of Electrical Engineering
University of Notre Dame






reply