Hello, I have a PDMS (Sylgard 184 from Dow Corning) device installed in a water flow. I now have the problem, that even when using degassed water, air bubbles settle on the surface of the PDMS. As all the acrylic glas around is clean, it seems to have something to do with the PDMS. If anyone knows a technique to avoid this problem, I would kindly ask him to give me an advice. I know that plasma-treatment is known to solve this problem, but unfortunately we cannot plasma-treat this device, so I am looking for some other way. Thanks a lot Sebastian Grosse