hi all,

  I am using Su-8 and frequently there are air bubbles left in the
film after spin coating. It is more serious with thicker films. I
tried to get rid of them by putting the pre-spinning resist-coated
wafer in vacuum dessicator, but the bubbles won't go. Anyone have
experience in this?