Hi, Try Engineering Plastics, Inc., in Westboro, Massachusetts. Their phone # is 508 366-4425, Fax 508 366-2575, email epi@ma.ultranet.com. They do custom work in teflon. -Charles King At 01:26 PM 3/2/98 -0500, you wrote: >Hello all, > >I'm trying to extend PFA Teflon handles for 3" carriers for use in 6" >chemical bathes. The largest handles that Flouroware sells would force me >to put my hand into the solution or drop the carrier a few inches. I'd >still need to retrieve it though and dropping it may crack wafers. > >Does anyone know of anyone who could weld extensions on the handles I >have to make them long enough? > >Thanks in advance, > >Mike > >Michael H. Beggans >New Jersey Institute of Technology (NJIT) >mhb3128@megahertz.njit.edu >973-642-7738 voice >973-596-5794 fax > > > > >