I am interested in acoustic microscopy and would like to know if anyone can supply any information about state of the art in fabricating a 1-mm diameter and 1-mm radius of curvature concave surface in [100] silicon, using some sort of dry or wet etching technique and ideally obtaining a very smooth (rmn roughness ~1-nm) surface and sphericity. Thanks. Thomas Wilson Marshall University Department of Physics